| Subject: | Re: another discussion point on coolant system corrosion |
| From: | David Beierl |
| Date: | Fri, 30 Jun 2006 16:13:04 -0400 |
At 12:00 PM 6/30/2006 -0700, Alistair Bell wrote: >The surface area of the sacrificial metal, Al, was much, much greater >than the "gaining " metal stainless. Imagine the corrosion if it were >the other way around, or imagine someone using aluminium pop rivets >in a stainless structure exposed to salt air or spray, the rivets >would be corroded away in no time. I've seen aluminum castings (aluminum cleat on anodized aluminum mast, s/s fastenings) burst apart because the corrosion products from the aluminum could no longer fit in the slack space of the mounting holes. -- David Beierl - Providence RI USA -- http://pws.prserv.net/synergy/Vanagon/ '84 Westy "Dutiful Passage," '85 GL "Poor Relation"