| Subject: | Re: Metal inserts slide out? Easy fix. |
| From: | Jake de Villiers |
| Date: | Wed, 2 Mar 2011 16:30:59 -0800 |
You forgot to allow for the metal insert on the back side. That, and Acrylite FF is much more brittle than the soft plastic the coolant tubes are made of. I still ain't worried about Dixie's tubes... ;) On Wed, Mar 2, 2011 at 3:31 PM, David Beierl <dbeierl@attglobal.net> wrote: > At 01:16 AM 3/1/2011, Jake de Villiers wrote: > >> Hmm. When I re-did Dixie's pipes I put a couple or three rivets into each >> insert after the heat and beat treatment. I really don't see how there >> could be any stress risers created in the holes since the rivets are a >> compressive force on the flat plastic. >> > > The plastic isn't flat, of course; it's a ~3/4" radius circle. But I was > curious about this so I did a little checking on a piece of 1/8" acrylic and > found the results interesting. Have a look at > https://picasaweb.google.com/dbeierl/StressInPlasticFromPopRiveting# . > I'd expect the effect to be more pronounced since the pipe isn't flat, but > the propagation distance to be less because of the material. > > Yours, > David > -- Jake 1984 Vanagon GL 1.9 WBX - 'The Grey Van' 1986 Westy Weekender/2.5 SOHC Subie - 'Dixie' Crescent Beach, BC www.thebassspa.com www.crescentbeachguitar.com http://subyjake.googlepages.com/mydixiedarlin%27
Have something to add on this topic today? Revive this thread in the forum »