| Subject: | <No subject> |
| From: | David Beierl |
| Date: | Wed, 7 Nov 2012 14:26:08 -0500 |
At 01:12 PM 11/7/2012, Pat wrote: >A variation is used on my copper plumbing pipes. I sure hope that stuff has >some structural integrity. A sweat-soldered joint has enormous surface area and a very thin layer of solder that's pulled into the joint by capillary action. I've never heard of a well-made one having a problem (doesn't mean it hasn't happened). Yours, David