| Subject: | Re: Cavitation corrosion/erosion |
| From: | Malcolm Holser |
| Date: | Sun, 3 May 1998 13:32:31 -0700 |
> >conductive fluid. Our Vanagons have Aluminum heads, iron cylinders > >and magnesium cases -- a real horror! > > Aluminum cases. The cases are aluminum, just like the type IV. Type I cases > were aluminum/magnesium alloy. Well, I was wrong (again). I had long assumed that the cases were magnesium, since they were so basically similar to the TypeI cases, and so unlike the TypeIV cases (I have one of these, too). So I went out and took a sample of my 1986 2.1L waterboxer, and tried to ignite it without much luck. I will believe. Again I have spoken too soon, assuming things I did not know for fact. Oh, well -- I do this a lot, and now know that none of the Vanagon cases are suitable for campouts. Thankfully I still have many junk typeI cases lying about for this use. Malcolm
Have something to add on this topic today? Revive this thread in the forum »